Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of NORYL GTX™ Resin NX0031 - Americas - (PPE+PA*) - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for NORYL GTX™ Resin NX0031 - Americas:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Noryl GTX datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informação do produto
NORYL GTX™ NX0031 resin is a non-reinforced alloy of PPE/PA. This conductive, injection moldable grade exhibits high heat resistance, excellent chemical resistance, and high impact resistance. NORYL NX0031 resin was designed for electrostatic painting and powder coating without the need for a conductive primer. This material can also be solvent painted and is an excellent for candidate for exterior, painted applications such as trim and fairings for outdoor vehicles, motorcycle, heavy truck, bus, personal watercraft, and marine. It is available only in black.

UL Yellow Card Link E121562-533883
Características de processamento/físicasValorUnidadeMétodo de ensaio
ISO Dados
Índice de fluidez volumétrico, MVR 8 cm³/10min ISO 1133
Temperatura 280 °C -
Carga 5 kg -
Condutividade térmica do fundido 0.22 W/(m K) -
Capacidade térmica específica do fundido 2200 J/(kg K) -
Temperatura de ejeção 130 °C -
ASTM Dados
Índice de fluidez, MFI 8 g/10min ASTM D 1238
Temperatura 280 °C -
Carga 5 kg -
Propriedades mecânicasValorUnidadeMétodo de ensaio
ISO Dados
Módulo de tração 2000 MPa ISO 527
Tensão no escoamento 50 MPa ISO 527
Deformação no escoamento 4 % ISO 527
Tensão na ruptura 48 MPa ISO 527
Deformação na ruptura 30 % ISO 527
Módulo de flexão 1900 MPa ISO 178
Res. impacto Charpy c/entalhe, +23°C 18 kJ/m² ISO 179/1eA
Res. impacto Charpy c/entalhe, -30°C 10 kJ/m² ISO 179/1eA
Res. impacto Izod c/entalhe, +23°C, 4mm 20 kJ/m² ISO 180/1A
Res. impacto Izod c/entalhe, -30°C, 4mm 10 kJ/m² ISO 180/1A
ASTM Dados
Módulo de tração 2250 MPa ASTM D 638
Resistência à tração no escoamento 52 MPa ASTM D 638
Resistência à tração na ruptura 48 MPa ASTM D 638
Alongamento no escoamento 5 % ASTM D 638
Deformação na ruptura 34 % ASTM D 638
Módulo de flexão 2100 MPa ASTM D 790
Impacto Izod com entalhe, 1/8 in 224 J/m ASTM D 256
Impacto Izod com entalhe, baixa temperatura 117 J/m ASTM D 256
Temperatura -30 °C -
Propriedades térmicasValorUnidadeMétodo de ensaio
ISO Dados
Temperatura de amolecimento Vicat, B 175 °C ISO 306
Temperatura de amolecimento Vicat, 120°C/h 50N 180 °C ISO 306
Coef. de expansão térmica linear, paralelo 100 E-6/K ISO 11359-1/-2
Coef. de expansão térmica linear, perpend. 90 E-6/K ISO 11359-1/-2
Flamabilidade a 1.5mm esp. nom. HB class IEC 60695-11-10
Espessuras do tubo de teste 1.5 mm -
ASTM Dados
DTUL @ 66 psi 176 °C ASTM D 648
DTUL @ 264 psi 136 °C ASTM D 648
Temperatura de amolecimento Vicat 175 °C ASTM D 1525
Outras propriedadesValorUnidadeMétodo de ensaio
Absorção de água 4.2 % Sim. to ISO 62
Absorção de umidade 1.2 % Sim. to ISO 62
Densidade 1090 kg/m³ ISO 1183
Densidade 1090 kg/m³ ASTM D 792
Recomendação de processamento Moldagem por injeçãoValorUnidadeMétodo de ensaio
Pré-secagem - temperatura 95 - 105 °C -
Pré-secagem - tempo 3 - 4 h -
Umidade do processamento ≤0.07 % -
Temperatura da massa 270 - 295 °C -
Temperatura do molde 65 - 95 °C -
Zona 1 255 - 295 °C -
Zona 2 260 - 295 °C -
Zona 3 265 - 295 °C -
Velocidade de parafuso 20 - 100 rpm -
Contrapressão 0.3 - 1.4 MPa -
Diagrama
Viscosidade - taxa de cisalhamento , NORYL GTX™  Resin NX0031 - Americas, (PPE+PA*), SABIC
Tensão de cisalhamento - taxa de cisalhamento , NORYL GTX™  Resin NX0031 - Americas, (PPE+PA*), SABIC
Volume específico - temperatura (pvT) , NORYL GTX™  Resin NX0031 - Americas, (PPE+PA*), SABIC
Características
Processamento
Moldagem por injeção
Disponibilidade regional
América do Norte
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.